Originální abstrakt

A rejuvenation process of a very old nickel-iron accumulator (about 75 years old) is described in this article. The supposed nominal parameters of the accumulator are 12V/(8Ah -10Ah). All cells of the accumulator were rejuvenated by a quite long and laborious process including 11 cycles of charging and discharging, several changing of the electrolyte and even using a deep discharging to improve the capacity of the negative iron electrode. The charging and discharging characteristics of all cells were measured during the rejuvenation.

Klíčová slova

NiFe cell, capacity, rejuvenation, charging charcacteristics, discharging characteristics, 1st plateau, 2nd plateau

Autoři

VOREL, P.; PROCHÁZKA, P.; PAZDERA, I.; ČERVINKA, D.

Rok RIV

2014

Vydáno

31. 8. 2014

ISBN

978-80-214-5008-0

Kniha

15th international conference ABAF

Strany od

100

Strany do

105

Strany počet

5

BibTex

@inproceedings{BUT110557,
  author="Pavel {Vorel} and Petr {Procházka} and Ivo {Pazdera} and Dalibor {Červinka}",
  title="Rejuvenation of a NiFe accumulator from 1930´s",
  booktitle="15th international conference ABAF",
  year="2014",
  pages="100--105",
  isbn="978-80-214-5008-0"
}