Metal matrix to ceramic matrix transition via feedstock processing of SPS titanium composites alloyed with high silicone content

TKACHENKO, S. ČÍŽEK, J. MUŠÁLEK, R. DVOŘÁK, K. SPOTZ, Z. MONTUFAR JIMENEZ, E. CHRÁSKA, T. KŘUPKA, I. ČELKO, L.

Originální název

Metal matrix to ceramic matrix transition via feedstock processing of SPS titanium composites alloyed with high silicone content

Typ

článek v časopise ve Web of Science, Jimp

Jazyk

angličtina

Originální abstrakt

Titanium silicides are promising candidates for use as a reinforcement in advanced light-weight composites due to their excellent mechanical properties and oxidation resistance at high temperatures, sufficient wear resistance, and high chemical stability in various corrosion environments. Direct in-situ synthesis of such composites from titanium-silicon (Ti-Si) powder feedstock by spark plasma sintering (SPS) was used in this study with a particular attention on the effect of the powder processing parameters (blending, co-milling, milling þ blending) on the microstructure formation and mechanical properties of the sintered composites. As opposed to the previous silicide-reinforced Ti studies, this was done for high silicone content (20 wt%). It was found that, despite the powders initial identical composition, the microstructure and phase content of the compacts varied significantly with the used powder fabrication route. Taking advantage of this, composites ranging from relatively soft metal-matrix (52 vol% metallic Ti; using non-milled Ti and coarse or fine-milled Si) to hard ceramic-matrix (11 vol% metallic Ti, using fine-dispersed joint-milled mixture of Ti and Si) were obtained. Due to in-situ formation of various TiSi2, TiSi, Ti5Si4 and Ti5Si3 silicide reinforcement phases contents with high hardness and stiffness, all the sintered composites showed superior hardness and wear resistance (an increase as much as 44) in comparison to pure Ti. Importantly, hardness and elastic modulus of intermediate compounds TiSi2, TiSi, Ti5Si4 and Ti5Si3 were measured using instrumented indentation technique for the first time and are presented in the paper.

Klíčová slova

Intermetallic-strengthened composites; Titanium silicides; Rapid sintering; Nanoindentation; Wear

Autoři

TKACHENKO, S.; ČÍŽEK, J.; MUŠÁLEK, R.; DVOŘÁK, K.; SPOTZ, Z.; MONTUFAR JIMENEZ, E.; CHRÁSKA, T.; KŘUPKA, I.; ČELKO, L.

Vydáno

15. 6. 2018

Nakladatel

Elsevier

Místo

Švýcarská konfederace

ISSN

0925-8388

Periodikum

Journal of Alloys and Compounds

Ročník

764

Číslo

1

Stát

Švýcarská konfederace

Strany od

776

Strany do

788

Strany počet

13

URL

Plný text v Digitální knihovně

BibTex

@article{BUT149203,
  author="Serhii {Tkachenko} and Jan {Čížek} and Radek {Mušálek} and Karel {Dvořák} and Zdeněk {Spotz} and Edgar Benjamin {Montufar Jimenez} and Tomáš {Chráska} and Ivan {Křupka} and Ladislav {Čelko}",
  title="Metal matrix to ceramic matrix transition via feedstock processing of SPS titanium composites alloyed with high silicone content",
  journal="Journal of Alloys and Compounds",
  year="2018",
  volume="764",
  number="1",
  pages="776--788",
  doi="10.1016/j.jallcom.2018.06.086",
  issn="0925-8388",
  url="https://doi.org/10.1016/j.jallcom.2018.06.086"
}