KLAKURKOVÁ, L. JULIŠ, M. ČELKO, L. HORYNOVÁ, M. HÉGR, E. ŠVEJCAR, J.
Originální název
Analysis of surface defects of aluminium components with hard anodized layers
Typ
článek v časopise ve Web of Science, Jimp
Jazyk
angličtina
Originální abstrakt
Final quality inspection regularly reveals surface defects on components after hard anodizing. The aim of the analysis was to identify the cause of the defects and unambiguously determine whether the defect is caused by the quality of the base material, manufacturing technology of the component, the heat treatment or by the final surface treatment technology (anodizing). Analysis of the chemical composition and hardness measurements were performed to eliminate the possibility of any errors during material selection and heat treatment process. The capillary test revealed two major defects and also small amount of minor defects. To determine cause of the defects, light and scanning electron microscopy including EDS chemical microanalysis was used. Detailed study of the major defect and EDS microanalysis of its interior confirmed existence of defect prior to coating formation. Further examination of the major defect and its surroundings led to conclusion, that the defect was formed during primary foundry processes when billet was manufactured.
Klíčová slova
Failure analysis; Hard anodizing; Rolling defects; Metallurgical investigation; Metallography
Autoři
KLAKURKOVÁ, L.; JULIŠ, M.; ČELKO, L.; HORYNOVÁ, M.; HÉGR, E.; ŠVEJCAR, J.
Rok RIV
2015
Vydáno
1. 10. 2015
Nakladatel
Elsevier
Místo
ISSN
1350-6307
Periodikum
ENGINEERING FAILURE ANALYSIS
Ročník
56
Číslo
1
Stát
Spojené království Velké Británie a Severního Irska
Strany od
300
Strany do
306
Strany počet
7
URL
http://dx.doi.org/10.1016/j.engfailanal.2015.01.013
BibTex
@article{BUT116567, author="Lenka {Klakurková} and Martin {Juliš} and Ladislav {Čelko} and Miroslava {Horynová} and Eduard {Hégr} and Jiří {Švejcar}", title="Analysis of surface defects of aluminium components with hard anodized layers", journal="ENGINEERING FAILURE ANALYSIS", year="2015", volume="56", number="1", pages="300--306", doi="10.1016/j.engfailanal.2015.01.013", issn="1350-6307", url="http://dx.doi.org/10.1016/j.engfailanal.2015.01.013" }